2013

/* 2013 */

  • Prize

  1. Honorable Mention (Ph. D. Category) in the 21st Rudy Scavuzzo Student Paper Symposium Competition at the 2013 ASME Pressure Vessels Piping Conference
    Nao Fujimura, Takashi Nakamura, Hiroyuki Oguma
    17. July 2013
    “Application of Surface Roughness Parameters to the Evaluation of Low
    Cycle Fatigue Damage in Austenitic Stainless Steel”
    American Society of Mechanical Engineering, ASME

    Fujimura

  2. 第31回疲労シンポジウム 優秀研究発表賞(学術分野)
    吉本健志
    2013年3月1日
    「人工微小欠陥を有するSNCM439の高サイクル疲労特性に及ぼす真空環境の影響」
    公益社団法人日本材料学会 疲労部門委員会 疲労発―第037号

Yoshimoto

 

  • Scientific Paper

  1. Ti-6Al-4V合金の表面および内部起点型疲労破壊における強度支配因子
    小熊博幸,中村 孝
    材料,Vol. 62,No. 12,p. 731-737 (2013)
  2. 表面粗さ測定に基づくSUS316NGの疲労損傷評価と適用範囲
    藤村奈央,中村 孝,小熊博幸,中島智広,信耕友樹
    材料,Vol. 62,No. 12,p. 750-755 (2013)
  3. 微小欠陥を有する高強度鋼の疲労特性に及ぼす真空環境の影響
    大岡武史,吉本健志,中村 孝
    日本機械学会論文集A編 Vol. 79,No. 806,p. 1545-1549 (2013)
    J-STAGE_logo
  4. Fatigue crack propagation properties of Ti–6Al–4V in vacuum environments
    H. Oguma, T. Nakamura
    International Journal of Fatigue, Vol. 50, p. 89–93 (2013)
    iconHUSCUP
  5. Changes in Surface roughness during Low Cycle Fatigue Process of Austenitic Stainless Steel
    Nao Fujimura, Takashi Nakamura, Hiroyuki Oguma
    Journal of Solid Mechanics and Materials Engineering, Vol. 7, No. 3, p. 372-380 (2013)
  • Others

  1.  【国内外トピックス】Technische Universität Kaiserslauternにおける在外研究
    小熊博幸
    材料,Vol. 62,No. 12,p. 792-793 (2013)
  • International Conference

  1. Effects of Strain Rate on the Very High Cycle Fatigue Properties of Low Alloy Steel SFVQ1A
    Takashi Nakamura, Hiroyuki Oguma, Shingo Nukaya
    PVP2013-97756, Proceedings of the ASME 2013 Pressure Vessels & Piping Conference (CD-ROM) (2013)
  2. Application of Surface Roughness Parameters to the Evaluation of Low Cycle Fatigue Damage in Austenitic Stainless Steel
    Nao Fujimura, Takashi Nakamura, Hiroyuki Oguma
    PVP2013-97887, Proceedings of the ASME 2013 Pressure Vessels & Piping Conference (CD-ROM) (2013)
  3. Fatigue properties of Ti alloy in vacuum environment
    Hiroyuki Oguma, Takashi Nakamura, Kazuaki Takaku
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 15 (2013)
  4. Very high cycle fatigue mechanisms of high strength materials
    Takashi Nakamura, Hiroyuki Oguma, Takeshi Ooka
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 20 (2013)
  5. Fatigue damage assessment of SUS316NG based on surface roughness measurement
    Nao Fujimura, Takashi Nakamura, Hiroyuki Oguma
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 33 (2013)
  6. Effects of vacuum environment on fatigue properties of high strength steel with a small defect
    Takeshi Ooka, Kenji Yoshimoto, Takashi Nakamura, Hirouki Oguma
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 36 (2013)
  7. A development of cyclic press method for nano-structural refinement of metal surface
    Masahiro Ueno, Takashi Nakamura, Kenji ookubo, Seiichi Watanabe
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 38 (2013)
  8. The detection of small internal fatigue cracks in Ti-6Al-4V by using synchrotron radiation μ CT imaging
    Shinya Nakayama, Takashi Nakamura, Hiroyuki Oguma
    The 3rd East Asia Mechanical and Aerospace Engineering Workshop
    p. 40 (2013)
  • Domestic Conference

  1. 放射光μCTイメージングを用いたTi-6Al-4V内部に発生する微小疲労き裂の検出
    中山慎也,中村 孝,小熊博幸,塩澤大輝,中井善一,上杉健太朗
    日本機械学会 M&M2013 材料力学カンファレンス
    OS1307,CD-ROM (2013)
  2. 表面に微小き裂を有するポリイミド薄膜材の破壊靭性
    鈴木千慶,中村 孝,小熊博幸
    日本機械学会 M&M2013 材料力学カンファレンス
    PS11,CD-ROM (2013)
  3. SUS316NGの低サイクル疲労における表面性状の変化
    新沼賢基,藤村奈央,信耕友樹,中村 孝,小熊博幸
    日本機械学会 M&M2013 材料力学カンファレンス
    PS15,CD-ROM (2013)
  4. SNCM439 の疲労特性におよぼす真空環境の影響
    吉中奎貴,中村 孝,小熊博幸
    日本機械学会北海道支部 第52回講演会 講演概要集
    No. 132-2,p. 11-12 (2013)
  5. Ti-6Al-4V 合金の破面様相に与える試験環境および負荷応力の影響
    髙久和明,中村 孝,小熊博幸
    日本機械学会北海道支部 第52回講演会 講演概要集
    No. 132-2,p. 13-14 (2013)
  6. 表面粗さに基づいたSUS316NG の低サイクル疲労損傷評価
    信耕友樹,藤村奈央,新沼賢基,中村 孝,小熊博幸
    日本機械学会北海道支部 第52回講演会 講演概要集
    No. 132-2,p. 15-16 (2013)
  7. PEEK-TiO2 ナノコンポジットの機械特性および耐UV 性に及ぼす TiO2微粒子の影響
    本村拓斗,中村 孝,小熊博幸,毛利徳光
    日本機械学会北海道支部 第52回講演会 講演概要集
    No. 132-2,p. 91-92 (2013)
  8. Cyclic Press 法によるS25C の表面微細化に及ぼす負荷繰返し数の影響
    中谷建太朗,植野正大,中村 孝,小熊博幸,大久保賢二,渡辺精一
    日本機械学会北海道支部 第52回講演会 講演概要集
    No. 132-2,p. 93-94 (2013)
  9. 耐紫外線性の向上を目的としたエポキシ/TiO2ナノコンポジットの試作
    中村 孝,静 宏幸,小熊博幸
    日本機械学会 2013年度年次大会大会
    J191026,DVD (2013)
  10. チタン合金の内部破壊における特異な破面領域の形成機構
    小熊博幸 中村 孝
    日本材料学会 第312回疲労部門委員会
    研究討論会資料 p. 1-10 (2013)
  11. 疲労き裂伝播下限界の欠陥寸法依存性に及ぼす真空環境の影響
    中村 孝,小熊博幸,吉本健志,大岡武史,吉中奎貴
    日本材料学会 第62期学術講演会講演論文集
    506,USB (2013)
  12. チタン合金の真空環境下で見られる特異な破面領域の形成因子
    小熊博幸,中村 孝,高久和明
    日本材料学会 第62期学術講演会講演論文集
    507,USB (2013)
  13. 表面粗さ計測に基づくSUS316NGの疲労損傷評価と適用範囲
    藤村奈央,小熊博幸,中村 孝,中島智広,信耕友樹
    日本材料学会 第62期学術講演会講演論文集
    515,USB (2013)